view【PRODUCT - Outline】 |
|
JX-107 series is a rosin-base high-solid content full dulling flux that provides excellent solder performance and high reliability for the Tin-Lead alloy,non-reflective solder joints surface can reduce worker eye strain during
inspection,Also can meet the requirement of no-cleaning process, Additionally,leaves low-tacky flux reside behind on the solder side after soldering.
|
view【Product - Features】 |
|
reduce bridging and solder balling
Smooth solder joints with full dulling
Evenly spread,low tack flux residue
Can be applied via spraying or foaming
|
view【Product - Technology Planning】 |
|
Technical Specifications
|
|
|
|
Ltem
|
JX-107
|
JX-107D
|
Reference Standard
|
Solder joint
|
dull
|
dull
|
\
|
Appearance
|
Pale Yellow Clear Liquid
|
Pale Yellow Clear Liquid
|
GB/9491-2002
|
Solids Content,wt/wt%
|
10-12
|
8-10
|
GB/9491-2002
|
SPECIFIC GRAVITY(20℃)
|
0.825±0.005
|
0.825±0.005
|
GB/9491-2002
|
HALIDE CONTENT,wt/wt%
|
0.15±0.05
|
≤0.05
|
GB/9491-2002
|
ACID VALUE(mgKOH/g)
|
35-40
|
35-40
|
GB/9491-2002
|
SPREAD FACTOR
|
≥80
|
≥80
|
GB/9491-2002
|
Copper plate corrosion
|
No evidence of corrosion
|
No evidence of corrosion
|
GB/9491-2002
|
SIR(40°C,90% RH)
|
≥1011Ω
|
≥1011Ω
|
GB/9491-2002
|
conductivity of aqueous extract
|
≥104
|
≥104
|
GB/9491-2002
|
|
view【Product - process parameters】 |
|
Technological Parameters
|
|
Bottom side Preheat Temperature
|
90-100°C
|
Conveyor Angle
|
4-7°
|
Conveyor Speed
|
1.2-1.7m/min
|
Contact Time in the Solder
|
2.0-3.0 sec
|
Solder Pot Temperatyre (Sn63/Pb37)
|
245-260°C
|
Application method
|
Spray or Foam
|
Recommended Thinner
|
JX-600
|
Recommended cleaner
|
JX-808
|
Shelf Life
|
12 months
|
|